FS108 liner filling material

FS108 liner filling material performance characteristics 1. Good fluidity, strong filling; 2. Conveni……

Related
message
detail
content details

FS108 liner filling material

Performance characteristics

1. Good fluidity, strong filling;

2. Convenient room temperature curing method;

3. Low shrinkage, good adhesion and high compressive strength after curing;

Product characteristics

It is used to fill the gap and seam of the main lining plate of the crusher, which can support the shaking caused by vibration, and play the role of noise reduction and buffering. It is also used to strengthen the structure of the cracks between the matrix and the matrix, and has good anti-seismic and wear-resistant characteristics.

Technical index

Mixed color

Mixed state

Density (g/cm3)

Compressive strength (MPa) GB/T 1041-2008

Shear strength (MPa) GB/T 1041-2008

Bending strength (MPa) GB/T 1041-2008

Hardness (Shors D) GB/T 241-2008

gray

liquid

1.63

120.0 or higher

22.0 or higher

18.5 or higher

86

Curing properties of FS1765 (test condition: room temperature)

 

Operating time

Operating temperature

Curing time

Full load curing time

Operating temperature

30min

5-30 ℃

15h

48h

-40℃ to 150℃


Usage method

1. Cleaning parts and preparation

All the surface to be poured must be cleaned, and there must be no dirt, grease and dust on the surface in contact with the colloid. In addition, seal the ring holes around the seam and the bottom with adhesive tape to prevent leakage; In winter and at low temperature, heating component A to 25-35℃ to reduce viscosity and facilitate pouring; In order to facilitate disassembly, oil or release agent can be pre-applied to the filling base.

2. Add glue

Fix the agitator on the low speed electric drill, turn on component A and stir for 1 minute, then introduce component B into component A and stir for 3 minutes. (Operation time: total time from mixing to filling, not more than 15 minutes)

3. Casting and curing

The mixed glue is injected along the end of the gap to be poured to facilitate the exhaust, and the glue with uneven color is not injected. After the filling of the pouring gap is completed, it is placed and cured for 12-24 hours, and the difference in temperature will affect the curing speed. Generally, 12 hours of curing in summer can be carried out, and 24 hours of curing can be carried out in winter.

 

Matters needing attention

1. The operating temperature of FS-1765 filling glue is 5-30℃, and the pouring gap is not within the temperature range.

 2. It is difficult to cast at low temperature, so component A can be heated to about 25℃ and then mixed;

 3. In the case of high temperature, the operation time needs to be reduced, and the mixed glue should be poured as soon as possible to avoid gel.

Storage and shelf life

Non-dangerous goods, stored in a cool and dry place, shelf life is 12 months;

Packing: 20kg/ group, plastic drum. 